1.Technical index

2.Product description of Super Intalox Ceramic Filler
3.Product dimensions and other physical indicators

4. Main features of the product
1) High acid and alkali resistance, acid resistance Greater than or equal to 99.8%, alkali resistance Greater than or equal to 85%
2) Low porosity, good density, high degree of porcelain transformation, porosity Less than or equal to 1.0%
3) The mode has high hardness and good wear resistance, with a Mohs hardness greater than 6.5
4) Low water absorption rate, strong sintering ability, water absorption rate Less than or equal to 0.1%
5) High flux, reduced pressure, high efficiency, effectively increasing gas channels and liquid distribution
5. Product application