Hydrophobic type calcium silicate board, also known as hydrophobic calcium silicate board, has no asbestos component, microporous structure and strong hydrophobic performance. After being immersed in water for 48 hours, its performance will not be affected. In particular, it has strong boiling water resistance. The product has fire resistance, heat insulation, aging resistance and corrosion resistance. The brand is TRR, which is commonly used in electric power, chemical industry and underwater engineering.
Gửi yêu cầu
Nói chuyện ngay
Mô tả

1,Product introduction of hydrophobic type calcium silicate board

The product is non asbestos hard insulation material with hydrophobic microporous structure. It has high temperature resistance of 650 degree , strong heat resistance, no deformation in the temperature range of use, high hydrophobicity, and can be soaked in water for a long time without affecting the use performance, especially strong boiling resistance. The product is weakly alkaline, combined with crystal, completely different from rock wool insulation material. The product has high compressive strength, stable thermal insulation structure, fireproof, heat insulation, weather resistance, aging resistance and corrosion resistance. The product is white inorganic material

2,Main technical parameter of Hydrophobic type calcium silicate board

Kg/m3

Less than or equal to 220

>0.3

>0.5

650

343±5 degree

W/m.k

0.06

923k,16h,%

Less than or equal to 1.5

%

Less than or equal to 7.5

%

>97,Soak in water for 48 hours without water seepage

3. Main features of the product

1) Fire performance: Class A, safety and environmental protection

2) High strength, it is the highest strength of inorganic insulation materials

3) The hydrophobic rate was more than 97%, and there was no change of water permeability after soaking in water for 48 h

4) Good thermal insulation, thermal conductivity is lower than other hard block insulation materials

5) Good weather resistance, no deformation within the temperature range

6) Environmental protection, asbestos free products, anti-bacterial, anti mildew, anti-aging, anti-corrosion

7) Light weight, arbitrary cutting, convenient for construction

4. Product specification: 600 * 400mm, 600 * 300mm, thickness 30-300mm

5. Application: widely used in electric power, chemical industry, metallurgy, boiler, kiln   

6,Our company promises to customers: to provide free technical exchanges and services with customers, and to provide samples to customers free of charge without any sample fees.

7,Achievements generated: Our company has previously shipped 150 tons to Korea.







Email:wp@cnjingganrefractory.com/sdwenping@163.com

TEL: 86-0533-4188518 / FAX: 86-0533-4188518 

Rose:+86-13275332819(wechat/whatsapp number)


Chú phổ biến:

Gửi yêu cầu
Liên hệ với chúng tôi
  • Điện thoại: +86-533-4188518
  • Mob: +8613275332819
  • E - Thư: sdwenping@163.com
  • Thêm: Phòng 711, Số 3, Yanhe Đường, Boshan, Zibo, Sơn Đông, Trung Quốc

(0/10)

clearall